Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %<= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545ASTM D2240
Tensile Strength 9.65 MPa1400 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Tensile Modulus 0.393 GPa57.0 ksiASTM D638
Flexural Strength 10.3 MPa1500 psiASTM D790
Flexural Modulus 0.200 GPa29.0 ksiASTM D790
Compressive Strength 9.65 MPa1400 psi10% Def.; ASTM D695
Compressive Modulus 0.372 GPa54.0 ksiASTM D695
Izod Impact, Notched NBNBASTM D256 Type A
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 118 °C244 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 71.1 °C160 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Flammability, UL94 HBHB1/8 inch (Estimated Rating)
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA YesYes
NSF NoNo
USDA YesYes
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak UnacceptableUnacceptable
Alcohols UnacceptableUnacceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak UnacceptableUnacceptable
Chlorinated Solvents UnacceptableUnacceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight UnacceptableUnacceptable
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic UnacceptableUnacceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Miscellaneous PropertiesMetricEnglishComments
Targeted Usage Structural UsesStructural Uses
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.