System Message
Searches:
Step-by-Step Selector
|
Quick Database Search
Mitsubishi Chemical Advanced Materials Duratron™ U2300 PEI Extruded 30% Glass Reinforced Polyetherimide
Categories:
Polymer
;
Thermoplastic
;
Polyetherimide (PEI)
;
Polyetherimide (PEI), 30% Glass Fiber
Material Notes:
Duratron™ U2300 PEI is a flame resistant Polyetherimide that is 30% glass-reinforced, allowing this grade to exhibit the highest rigidity, strength, dimensional stability, and heat resistance of all Duratron™ PEI shapes.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Metric
English
Comments
Specific Gravity
1.51
g/cc
1.51
g/cc
ASTM D792
Water Absorption at Saturation
0.900 %
0.900 %
ASTM D570 (17)
Electrical Properties
Metric
English
Comments
Surface Resistivity per Square
1.00e+14
ohm
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
3.70
@Frequency 1.00e+6 Hz
3.70
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength
30.3
kV/mm
770
kV/in
ASTM D149
Dissipation Factor
0.00150
@Frequency 1.00e+6 Hz
0.00150
@Frequency 1.00e+6 Hz
ASTM D150
Thermal Properties
Metric
English
Comments
CTE, linear
19.8
µm/m-°C
11.0
µin/in-°F
ASTM E-831 (TMA)
Thermal Conductivity
0.225
W/m-K
1.56
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
171
°C
340
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
210
°C
410
°F
ASTM D648
Glass Transition Temp, Tg
210
°C
410
°F
DMA- Tan d
Chemical Resistance Properties
Metric
English
Comments
Acids, Strong (pH 1-3)
Limited
Limited
Acids, Weak
Acceptable
Acceptable
Alcohols
Acceptable
Acceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Unacceptable
Alkalies, Weak
Acceptable
Acceptable
Chlorinated Solvents
Unacceptable
Unacceptable
Continuous Sunlight
Acceptable
Acceptable
Hot Water / Steam
Acceptable
Acceptable
Hydrocarbons - Aliphatic
Limited
Limited
Hydrocarbons - Aromatic
Unacceptable
Unacceptable
Inorganic Salt Solutions
Acceptable
Acceptable
Ketones, Esters
Unacceptable
Unacceptable
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
P1SM51 / 20147