Mitsubishi Chemical Advanced Materials Acetron™ VMX FG POM-C Food Grade Polyoxymethylene
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: A copolymer acetal specifically designed for use in food processing and packaging where it can easily be traced by different detection systems installed to detect physical contamination.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.63 g/cc1.63 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 79.079.0ASTM D785
Tensile Strength 55.0 MPa7980 psiISO 527-1/-2 (7)
Elongation at Yield 14.0 %14.0 %ISO 527-1/-2 (7)
Compressive Yield Strength  25.0 MPa
@Strain 1.00 %
3630 psi
@Strain 1.00 %
ISO 604 (10)
 44.0 MPa
@Strain 2.00 %
6380 psi
@Strain 2.00 %
ISO 604 (10)
 75.0 MPa
@Strain 5.00 %
10900 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 122 µm/m-°C68.0 µin/in-°FASTM E-831 (TMA)
 125 µm/m-°C
@Temperature 23.0 - 60.0 °C
69.4 µin/in-°F
@Temperature 73.4 - 140 °F
 160 µm/m-°C
@Temperature 23.0 - 100 °C
88.9 µin/in-°F
@Temperature 73.4 - 212 °F
Melting Point 169 °C336 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.