Material Notes: Life Science Grade PEI stock shapes made from unfilled ULTEM™ PEI resin. Pre-assessed for biocompatibility on both resin and shape for up to 24 hours contact with body tissue according to USP VI and ISO 10993. Outstanding mechanical, thermal, and electrical performance, plus very good chemical and hydrolysis resistance. Suitable for repeated sterilization via all current methods.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.28 g/cc1.28 g/ccASTM D792
Water Absorption at Saturation 1.25 %1.25 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 115115ASTM D785
Hardness, Shore D 85.085.0ISO 868
Tensile Strength 129 MPa18700 psiISO 527-1/-2 (7)
Elongation at Yield 7.00 %7.00 %ISO 527-1/-2 (7)
Flexural Strength 167 MPa24200 psiISO 178 (12)
Compressive Yield Strength  31.0 MPa
@Strain 1.00 %
4500 psi
@Strain 1.00 %
ISO 604 (10)
 61.0 MPa
@Strain 2.00 %
8850 psi
@Strain 2.00 %
ISO 604 (10)
 137 MPa
@Strain 5.00 %
19900 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 97.0 MPa14100 psiASTM D732
Charpy Impact, Notched 0.350 J/cm²1.67 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.15
@Frequency 1.00e+6 Hz
3.15
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243-1 (15)
 32.7 kV/mm830 kV/inASTM D149
Dissipation Factor 0.00130
@Frequency 1.00e+6 Hz
0.00130
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C31.0 µin/in-°FASTM E-831 (TMA)
 50.0 µm/m-°C
@Temperature 23.0 - 100 °C
27.8 µin/in-°F
@Temperature 73.4 - 212 °F
 50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
 60.0 µm/m-°C
@Temperature >=150 °C
33.3 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.177 W/m-K1.23 BTU-in/hr-ft²-°F
 0.240 W/m-K1.67 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 171 °C340 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 204 °C400 °FASTM D648
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Glass Transition Temp, Tg 210 °C410 °FDMA- Tan d
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic LimitedLimited
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM923 / 291080