Material Notes: Life Science Grade PC stock shapes, made from unfilled PC resin. Pre-assessed for biocompatibility on stock shape for up to 24 hours contact with body tissue according to USP VI and ISO 10993 and wetted contact applications in bioprocessing. Outstanding impact resistance, toughness, and dielectric properties, as well as very good mechanical and thermal properties. Good resistance to sterilization via EtO, plasma, gamma- & X-ray irradiation. Not suitable for steam sterilization.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption at Saturation 0.400 %0.400 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 75.075.0ASTM D785
Hardness, Shore D 79.079.0ISO 868
Tensile Strength 74.0 MPa10700 psiISO 527-1/-2 (7)
Elongation at Yield 6.00 %6.00 %ISO 527-1/-2 (7)
Flexural Strength 103 MPa14900 psiISO 178 (12)
Compressive Yield Strength  22.0 MPa
@Strain 1.00 %
3190 psi
@Strain 1.00 %
ISO 604 (10)
 40.0 MPa
@Strain 2.00 %
5800 psi
@Strain 2.00 %
ISO 604 (10)
 80.0 MPa
@Strain 5.00 %
11600 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 63.0 MPa9140 psiASTM D732
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.17
@Frequency 1.00e+6 Hz
3.17
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm400 kV/inASTM D149
 28.0 kV/mm711 kV/inIEC 60243-1 (15)
Dissipation Factor 0.000900
@Frequency 1.00e+6 Hz
0.000900
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.2 µm/m-°C39.0 µin/in-°FASTM E-831 (TMA)
 65.0 µm/m-°C
@Temperature 23.0 - 100 °C
36.1 µin/in-°F
@Temperature 73.4 - 212 °F
 65.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.186 W/m-K1.29 BTU-in/hr-ft²-°F
 0.210 W/m-K1.46 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C250 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 143 °C290 °FASTM D648
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Glass Transition Temp, Tg 145 °C293 °FDMA- Tan d
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.