Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 72.072.0ISO 868
Tensile Strength 34.0 MPa4930 psiISO 527-1/-2 (7)
Elongation at Yield 6.00 %6.00 %ISO 527-1/-2 (7)
Flexural Strength 50.0 MPa7250 psiISO 178 (12)
Compressive Yield Strength  18.0 MPa
@Strain 1.00 %
2610 psi
@Strain 1.00 %
ISO 604 (10)
 27.0 MPa
@Strain 2.00 %
3920 psi
@Strain 2.00 %
ISO 604 (10)
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+15 ohm1.00e+15 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 77.4 µm/m-°C43.0 µin/in-°FASTM E-831 (TMA)
 150 µm/m-°C
@Temperature 23.0 - 100 °C
83.3 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°F
Melting Point 164 °C327 °FASTM D3418
Maximum Service Temperature, Air 87.8 °C190 °FContinuous Use Temperature in Air after 20000 hr
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
NSF YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.