Mitsubishi Chemical Advanced Materials Proteus™ LSG HS PP-H Heat Stabilized Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Life Science Grade, Heat Stabilized PP-H stock shapes, made from high purity homopolymer polypropylene resin. Shapes are pre-assessed for biocompatibility at the stock shape level (USP VI & ISO 10993) and are supported for use in non-body contact medical applications. Exhibits superior resistance to steam sterilization, cleaning agents, and disinfectants over standard PP materials, and has improved dimensional stability.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 38.0 MPa5510 psiISO 527-1/-2 (7)
Elongation at Yield 6.00 %6.00 %ISO 527-1/-2 (7)
Flexural Strength 54.0 MPa7830 psiISO 178 (12)
Compressive Yield Strength  15.0 MPa
@Strain 1.00 %
2180 psi
@Strain 1.00 %
ISO 604 (10)
 27.0 MPa
@Strain 2.00 %
3920 psi
@Strain 2.00 %
ISO 604 (10)
 46.0 MPa
@Strain 5.00 %
6670 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 0.640 J/cm²3.05 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 108 µm/m-°C60.0 µin/in-°FASTM E-831 (TMA)
Melting Point 164 °C327 °FASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FContinuous Use Temperature in Air after 20000 hr
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SMP66m / 108908