Physical PropertiesMetricEnglishComments
Specific Gravity 1.31 g/cc1.31 g/ccASTM D792
Water Absorption at Saturation 0.500 %0.500 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 90.0 MPa13100 psiASTM D732
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.30
@Frequency 1.00e+6 Hz
3.30
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 18.9 kV/mm480 kV/inASTM D149
Dissipation Factor 0.00300
@Frequency 1.00e+6 Hz
0.00300
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C26.0 µin/in-°FASTM E-831 (TMA)
Thermal Conductivity 0.252 W/m-K1.75 BTU-in/hr-ft²-°F
Melting Point 340 °C644 °FASTM D3418
Maximum Service Temperature, Air 249 °C480 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D648
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.