Material Notes: |
This internally lubricated, glass-fiber reinforced PPS bridges the gap in performance and price between standard and advanced engineering plastics, exhibiting excellent resistance to wear, hydrolysis, and chemicals, as well as great electrical insulation and low flammability.
|