CTE, linearMetricEnglishComments
 103 µm/m-°C57.0 µin/in-°FASTM E-831 (TMA)
 85.0 µm/m-°C
@Temperature 23.0 - 100 °C
47.2 µin/in-°F
@Temperature 73.4 - 212 °F
 90.0 µm/m-°C
@Temperature 23.0 - 150 °C
50.0 µin/in-°F
@Temperature 73.4 - 302 °F
 155 µm/m-°C
@Temperature >=150 °C
86.1 µin/in-°F
@Temperature >=302 °F