Compressive Yield StrengthMetricEnglishComments
 30.0 MPa
@Strain 1.00 %
4350 psi
@Strain 1.00 %
ISO 604 (10)
 60.0 MPa
@Strain 2.00 %
8700 psi
@Strain 2.00 %
ISO 604 (10)
 99.0 MPa
@Strain 5.00 %
14400 psi
@Strain 5.00 %
ISO 604 (10)