CTE, linear
Metric
English
Comments
45.0 µm/m-°C
25.0 µin/in-°F
ASTM E-831 (TMA)
50.0 µm/m-°C
@Temperature 23.0 - 100 °C
27.8 µin/in-°F
@Temperature 73.4 - 212 °F
55.0 µm/m-°C
@Temperature 23.0 - 150 °C
30.6 µin/in-°F
@Temperature 73.4 - 302 °F
85.0 µm/m-°C
@Temperature >=150 °C
47.2 µin/in-°F
@Temperature >=302 °F