Compressive Yield Strength
Metric
English
Comments
40.0 MPa
@Strain 1.00 %
5800 psi
@Strain 1.00 %
ISO 604 (10)
79.0 MPa
@Strain 2.00 %
11500 psi
@Strain 2.00 %
ISO 604 (10)
143 MPa
@Strain 5.00 %
20700 psi
@Strain 5.00 %
ISO 604 (10)