Searches:   Step-by-Step Selector  | Quick Database Search
Ensinger PEI

<< Back to datasheet

Metric English
( This graph is merely a visual representation of the tabular data. It is not meant to predict any property behavior between data points.
Sample and/or test conditions are not necessarily identical for every data point; please note any comments beside any data points for details. )

Graph data in tabular format:
Compressive Yield StrengthMetricEnglishComments
 49.0 MPa
@Strain 1.00 %
7110 psi
@Strain 1.00 %
ISO 604 (10)
 91.0 MPa
@Strain 2.00 %
13200 psi
@Strain 2.00 %
ISO 604 (10)
 146 MPa
@Strain 5.00 %
21200 psi
@Strain 5.00 %
ISO 604 (10)