Compressive Yield StrengthMetricEnglishComments
 33.0 MPa
@Strain 1.00 %
4790 psi
@Strain 1.00 %
ISO 604 (10)
 68.0 MPa
@Strain 2.00 %
9860 psi
@Strain 2.00 %
ISO 604 (10)
 147 MPa
@Strain 5.00 %
21300 psi
@Strain 5.00 %
ISO 604 (10)