Compressive Yield StrengthMetricEnglishComments
 39.0 MPa
@Strain 1.00 %
5660 psi
@Strain 1.00 %
ISO 604 (10)
 77.0 MPa
@Strain 2.00 %
11200 psi
@Strain 2.00 %
ISO 604 (10)
 122 MPa
@Strain 5.00 %
17700 psi
@Strain 5.00 %
ISO 604 (10)