Mitsubishi Chemical Advanced Materials Nylatron™ WP PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Nylatron™ WP PA6 self-lubricated shapes outperform competing nylon products in wear resistance and load bearing capabilities, and also provide users with an economical solution across a wide range of applications and industries.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Water Absorption at Saturation 7.00 %7.00 %ASTM D570 (17)
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 99.0 µm/m-°C55.0 µin/in-°FASTM E-831 (TMA)
Thermal Conductivity 0.342 W/m-K2.37 BTU-in/hr-ft²-°F
Melting Point 216 °C420 °FASTM D3418
Maximum Service Temperature, Air 93.3 °C200 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FASTM D648
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak LimitedLimited
Alcohols LimitedLimited
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents LimitedLimited
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Targeted Usage Load + BearingLoad + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.