System Message
Searches:
Step-by-Step Selector
|
Quick Database Search
(Viewing data as-entered.
Click here
to return)
Mitsubishi Chemical Advanced Materials Altron™ PC Extruded, Unfilled, Polycarbonate
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Extruded
Material Notes:
A transparent, amorphous thermoplastic that offers superior impact strength and elasticity, minimal moisture absorption, excellent electrical properties, and outstanding resistance to acidic solutions.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
1.20
g/cc
ASTM D792
Water Absorption at Saturation
0.400 %
ASTM D570 (17)
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
75.0
ASTM D785
Hardness, Shore D
79.0
ISO 868
Tensile Strength
74.0
MPa
ISO 527-1/-2 (7)
Elongation at Yield
6.00 %
ISO 527-1/-2 (7)
Flexural Strength
103
MPa
ISO 178 (12)
Compressive Yield Strength
21.0
MPa
@Strain 1.00 %
ISO 604 (10)
40.0
MPa
@Strain 2.00 %
ISO 604 (10)
80.0
MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength
63.0
MPa
ASTM D732
Charpy Impact, Notched
9.00
kJ/m²
ISO 179-1/1eA
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
3.17
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength
28.0
kV/mm
IEC 60243-1 (15)
400
kV/in
ASTM D149
Dissipation Factor
0.000900
@Frequency 1.00e+6 Hz
ASTM D150
Thermal Properties
Original Value
Comments
CTE, linear
39.0
µin/in-°F
ASTM E-831 (TMA)
65.0
µm/m-°C
@Temperature 23.0 - 100 °C
65.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity
0.210
W/m-K
1.29
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
250
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
290
°F
ASTM D648
Minimum Service Temperature, Air
-50.0
°C
Glass Transition Temp, Tg
293
°F
DMA- Tan d
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Limited
Acids, Weak
Acceptable
Alcohols
Acceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Alkalies, Weak
Limited
Chlorinated Solvents
Acceptable
Continuous Sunlight
Limited
Hot Water / Steam
Limited
Hydrocarbons - Aliphatic
Acceptable
Hydrocarbons - Aromatic
Acceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Acceptable
Miscellaneous Properties
Original Value
Comments
Data Sheet Region
Americas
Targeted Usage
Structural Uses
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
P1SM10B / 20086