System Message
Searches:
Step-by-Step Selector
|
Quick Database Search
(Viewing data as-entered.
Click here
to return)
Mitsubishi Chemical Advanced Materials Ketron™ CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyetheretherketone (PEEK)
;
Polyetheretherketone, PEEK, Glass Fiber Filled
Material Notes:
A compression molded, 30% carbon fiber-reinforced polyetherether ketone that exhibits outstanding impact, corrosion, chemical, and wear resistance.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
1.42
g/cc
ASTM D792
Water Absorption at Saturation
0.500 %
ASTM D570 (17)
Mechanical Properties
Original Value
Comments
Shear Strength
76.0
MPa
ASTM D732
Thermal Properties
Original Value
Comments
CTE, linear
23.0
µin/in-°F
ASTM E-831 (TMA)
Thermal Conductivity
6.37
BTU-in/hr-ft²-°F
Melting Point
644
°F
ASTM D3418
Maximum Service Temperature, Air
480
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
450
°F
ASTM D648
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Limited
Acids, Weak
Acceptable
Alcohols
Acceptable
Alkalies, Strong (pH 11-14)
Acceptable
Alkalies, Weak
Acceptable
Chlorinated Solvents
Acceptable
Continuous Sunlight
Limited
Hot Water / Steam
Acceptable
Hydrocarbons - Aliphatic
Acceptable
Hydrocarbons - Aromatic
Acceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Acceptable
Miscellaneous Properties
Original Value
Comments
Data Sheet Region
Americas
Targeted Usage
Load + Bearing
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.