Mitsubishi Chemical Advanced Materials Fluorosint™ MT-01 PTFE reinforced with carbon fibers and organometallic fillers
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Carbon Fiber Filled

Material Notes: Fluorosint™ MT-01 is an extreme PTFE grade that was specifically developed for engineering applications where the low-friction and high-temperature benefits of PTFE-based materials also require outstanding strength, stiffness, and stability.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.27 g/cc2.27 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 74.074.0ASTM D785
Hardness, Shore D 70.070.0ISO 868
Tensile Strength 14.0 MPa2030 psiISO 527-1/-2 (7)
Elongation at Yield 6.00 %6.00 %ISO 527-1/-2 (7)
Flexural Strength 20.0 MPa2900 psiISO 178 (12)
Compressive Yield Strength  11.0 MPa
@Strain 1.00 %
1600 psi
@Strain 1.00 %
ISO 604 (10)
 17.0 MPa
@Strain 2.00 %
2470 psi
@Strain 2.00 %
ISO 604 (10)
 29.0 MPa
@Strain 5.00 %
4210 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 18.0 MPa2610 psiASTM D732
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+6 ohm1.00e+6 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C30.0 µin/in-°FASTM E-831 (TMA)
 60.0 µm/m-°C
@Temperature 23.0 - 100 °C
33.3 µin/in-°F
@Temperature 73.4 - 212 °F
 65.0 µm/m-°C
@Temperature 23.0 - 150 °C
36.1 µin/in-°F
@Temperature 73.4 - 302 °F
 100 µm/m-°C
@Temperature >=150 °C
55.6 µin/in-°F
@Temperature >=302 °F
Maximum Service Temperature, Air 260 °C500 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 93.3 °C200 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Structural UsesStructural Uses
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.