Mitsubishi Chemical Advanced Materials TIVAR™ DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized
Categories: Polymer; Thermoplastic; Polyethylene (PE); UHMW-PE

Material Notes: With an internal lubricant built into the polymer matrix with higher molecular weight, this premium UHMW-PE offers a lower coefficient of friction and enhanced wear and abrasion resistance vs. TIVAR™ 1000 UHMW-PE.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 59.0ISO 868
 59.0ISO 868
Tensile Strength 18.0 MPaISO 527-1/-2 (7)
Elongation at Yield 20.0 %ISO 527-1/-2 (7)
Flexural Strength 16.0 MPaISO 178 (12)
Compressive Yield Strength 6.00 MPa
@Strain 1.00 %
ISO 604 (10)
 10.0 MPa
@Strain 2.00 %
ISO 604 (10)
 10.0 MPa
@Strain 2.00 %
ISO 604 (10)
 16.0 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 22.0 MPaASTM D732
Charpy Impact, Notched 100 kJ/m²Partial Break; ISO 179-1/1eA
 130 kJ/m²Double Notched
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 1.00e+9 ohmANSI/ESD STM 11.11
 <= 1.00e+9 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µin/in-°FASTM E-831 (TMA)
 200 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.400 W/m-K
Melting Point 275 °FASTM D3418
Maximum Service Temperature, Air 180 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 116 °FASTM D648
Minimum Service Temperature, Air -238 °F
 -150 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Acceptable
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Miscellaneous PropertiesOriginal ValueComments
Data Sheet Region Americas
Targeted Usage Load + Bearing
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.