Searches:   Step-by-Step Selector  | Quick Database Search

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials QuickSilver™ HD (Heavy Duty) UHMW-PE, Premium Truck Lining
Categories: Polymer; Thermoplastic; Polyethylene (PE); UHMW-PE

Material Notes: Heavy duty bed liners that protect the integrity of original truck beds and improve the release of materials for quicker unloading, greater safety, and less carryback.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 49.0ASTM D785
Hardness, Shore D 62.0ISO 868
Tensile Strength 19.0 MPaISO 527-1/-2 (7)
Elongation at Yield 30.0 %ISO 527-1/-2 (7)
Flexural Strength 18.0 MPaISO 178 (12)
Compressive Yield Strength 6.50 MPa
@Strain 1.00 %
ISO 604 (10)
 10.0 MPa
@Strain 2.00 %
ISO 604 (10)
 16.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 80.0 kJ/m²Double Notched
 99.0 kJ/m²Partial Break; ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+13 ohmANSI/ESD STM 11.11
Dielectric Constant 2.30
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 2300 kV/inASTM D149
Dissipation Factor 0.000500
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µin/in-°FASTM E-831 (TMA)
 200 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.400 W/m-K
 2.84 BTU-in/hr-ft²-°F
Melting Point 275 °FASTM D3418
Maximum Service Temperature, Air 180 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 116 °FASTM D648
Minimum Service Temperature, Air -150 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Miscellaneous PropertiesOriginal ValueComments
Data Sheet Region Americas
Targeted Usage Load + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SMP14c / 210240