Mitsubishi Chemical Advanced Materials Duratron™ U2100 PEI Extruded 10% Glass Reinforced Polyetherimide
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 20% Glass Fiber

Material Notes: 10% glass-reinforced PEI shapes with great rigidity and dimensional stability as well as a low coefficient of linear thermal expansion.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Water Absorption at Saturation 1.00 %ASTM D570 (17)
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 340 °FContinuous Use Temperature in Air after 20000 hr
Glass Transition Temp, Tg 410 °FDMA- Tan d
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Continuous Sunlight Acceptable
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Limited
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.