Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
Categories:
Polymer
;
Thermoplastic
;
Polyketone
;
Polyetheretherketone (PEEK)
;
Polyetheretherketone, PEEK, Glass Fiber Filled
Material Notes:
An extruded, 30% glass fiber reinforced grade PEEK with excellent dimensional stability and outstanding chemical, corrosion, and creep resistance.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Metric
English
Comments
Specific Gravity
1.51
g/cc
1.51
g/cc
ASTM D792
Water Absorption at Saturation
0.300 %
0.300 %
ASTM D570 (17)
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
100
100
ASTM D785
Hardness, Shore D
87.0
87.0
ISO 868
Tensile Strength
80.0
MPa
11600
psi
ISO 527-1/-2 (7)
Elongation at Yield
4.00 %
4.00 %
ISO 527-1/-2 (7)
Flexural Strength
155
MPa
22500
psi
ISO 178 (12)
Compressive Yield Strength
54.0
MPa
@Strain 1.00 %
7830
psi
@Strain 1.00 %
ISO 604 (10)
103
MPa
@Strain 2.00 %
14900
psi
@Strain 2.00 %
ISO 604 (10)
155
MPa
@Strain 5.00 %
22500
psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength
97.0
MPa
14100
psi
ASTM D732
Charpy Impact, Notched
0.300
J/cm²
1.43
ft-lb/in²
ISO 179-1/1eA
Electrical Properties
Metric
English
Comments
Surface Resistivity per Square
1.00e+14
ohm
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Strength
19.7
kV/mm
500
kV/in
ASTM D149
24.0
kV/mm
610
kV/in
IEC 60243-1 (15)
Thermal Properties
Metric
English
Comments
CTE, linear
21.6
µm/m-°C
12.0
µin/in-°F
ASTM E-831 (TMA)
30.0
µm/m-°C
@Temperature 23.0 - 100 °C
16.7
µin/in-°F
@Temperature 73.4 - 212 °F
30.0
µm/m-°C
@Temperature 23.0 - 150 °C
16.7
µin/in-°F
@Temperature 73.4 - 302 °F
65.0
µm/m-°C
@Temperature >=150 °C
36.1
µin/in-°F
@Temperature >=302 °F
Thermal Conductivity
0.429
W/m-K
2.98
BTU-in/hr-ft²-°F
0.430
W/m-K
2.98
BTU-in/hr-ft²-°F
Melting Point
340
°C
644
°F
ASTM D3418
Maximum Service Temperature, Air
249
°C
480
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
232
°C
450
°F
ASTM D648
Minimum Service Temperature, Air
-20.0
°C
-4.00
°F
Chemical Resistance Properties
Metric
English
Comments
Acids, Strong (pH 1-3)
Limited
Limited
Acids, Weak
Acceptable
Acceptable
Alcohols
Acceptable
Acceptable
Alkalies, Strong (pH 11-14)
Acceptable
Acceptable
Alkalies, Weak
Acceptable
Acceptable
Chlorinated Solvents
Acceptable
Acceptable
Continuous Sunlight
Limited
Limited
Hot Water / Steam
Acceptable
Acceptable
Hydrocarbons - Aliphatic
Acceptable
Acceptable
Hydrocarbons - Aromatic
Acceptable
Acceptable
Inorganic Salt Solutions
Acceptable
Acceptable
Ketones, Esters
Acceptable
Acceptable
Miscellaneous Properties
Metric
English
Comments
Data Sheet Region
Americas
Americas
Targeted Usage
Structural Uses
Structural Uses
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
P1SM16 / 20094