Searches:   Step-by-Step Selector  | Quick Database Search

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ertalyte™ PET Polyester-semi-crystalline thermoplastic, extruded
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PET-P Polyester, Extruded

Material Notes: An unreinforced, semi-crystalline PET with excellent wear resistance, high strength, and compatibility with moderately acidic solutions. This grade is capable of sustaining high loads, and retains more of its original strength up to 180° F / 85° C than nylons or acetals.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Water Absorption at Saturation 0.900 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 96.0ASTM D785
Hardness, Shore D 80.0ISO 868
Tensile Strength 90.0 MPaISO 527-1/-2 (7)
Elongation at Yield 4.00 %ISO 527-1/-2 (7)
Flexural Strength 135 MPaISO 178 (12)
Compressive Yield Strength 33.0 MPa
@Strain 1.00 %
ISO 604 (10)
 64.0 MPa
@Strain 2.00 %
ISO 604 (10)
 107 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 55.0 MPaASTM D732
Charpy Impact, Notched 2.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.40
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 22.0 kV/mmIEC 60243-1 (15)
 385 kV/inASTM D149
Dissipation Factor 0.0200
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µin/in-°FASTM E-831 (TMA)
 60.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 80.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.290 W/m-K
 2.00 BTU-in/hr-ft²-°F
Melting Point 491 °FASTM D3418
Maximum Service Temperature, Air 210 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 240 °FASTM D648
Minimum Service Temperature, Air -20.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Unacceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Miscellaneous PropertiesOriginal ValueComments
Data Sheet Region Americas
Targeted Usage Load + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM07 / 20078