Mitsubishi Chemical Advanced Materials Duratron™ U2200 PEI Extruded 20% Glass Reinforced Polyetherimide
Categories:
Polymer
;
Thermoplastic
;
Polyetherimide (PEI)
;
Polyetherimide (PEI), 20% Glass Fiber
Material Notes:
Duratron™ U2200 PEI Polyetherimide shapes are 20% glass-reinforced, giving them exceptional rigidity and dimensional stability, high temperature resistance, and a low CLTE.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
1.41
g/cc
ASTM D792
Water Absorption at Saturation
1.00 %
ASTM D570 (17)
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
1.00e+14
ohm
ANSI/ESD STM 11.11
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
340
°F
Continuous Use Temperature in Air after 20000 hr
Glass Transition Temp, Tg
410
°F
DMA- Tan d
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Limited
Acids, Weak
Acceptable
Alcohols
Acceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Alkalies, Weak
Acceptable
Chlorinated Solvents
Unacceptable
Continuous Sunlight
Acceptable
Hot Water / Steam
Acceptable
Hydrocarbons - Aliphatic
Limited
Hydrocarbons - Aromatic
Unacceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Unacceptable
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.