Mitsubishi Chemical Advanced Materials Nylatron™ 66 SA FR PA66 Nylon 66, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: This flame-retardant nylon developed to fulfill UL94-V0 requirements for plastic flammability ratings. This nylon 66 is often used in transport and railway applications.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 87.0ASTM D785
Tensile Strength 79.0 MPaISO 527-1/-2 (7)
Elongation at Yield 7.00 %ISO 527-1/-2 (7)
Compressive Yield Strength 35.0 MPa
@Strain 1.00 %
ISO 604 (10)
 65.0 MPa
@Strain 2.00 %
ISO 604 (10)
 98.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 3.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 18.0 kV/mmIEC 60243-1 (15)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
Thermal Conductivity 0.370 W/m-K
Minimum Service Temperature, Air -30.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.