Material Notes: |
Nylon shapes that are fire, smoke, and toxicity retardant, enabling them to withstand temperatures up to 347° F / 175° C. The first engineering plastic to achieve JAR / FAR 25.853 compliance, this polyimide grade was developed specifically for use in aircraft interior environments.
|