Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57.0ISO 868
Tensile Strength 20.0 MPaISO 527-1/-2 (7)
Flexural Strength 19.0 MPaISO 178 (12)
Compressive Yield Strength 4.00 MPa
@Strain 1.00 %
ISO 604 (10)
 14.0 MPa
@Strain 2.00 %
ISO 604 (10)
 20.0 MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 90.0 kJ/m²Partial Break; ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
@Temperature 23.0 - 60.0 °C
Minimum Service Temperature, Air -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.