Searches:   Step-by-Step Selector  | Quick Database Search

Mitsubishi Chemical Advanced Materials TIVAR™ SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant
Categories: Polymer; Thermoplastic; Polyethylene (PE); UHMW-PE

Material Notes: TIVAR™ SuperPlus is a wear optimized, partially cross-linked UHMW-PE material with extremely high degree of polymerization for use in most demanding applications and environments.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 58.058.0ISO 868
Tensile Strength 17.0 MPa2470 psiISO 527-1/-2 (7)
Elongation at Yield 20.0 %20.0 %ISO 527-1/-2 (7)
Flexural Strength 15.0 MPa2180 psiISO 178 (12)
Compressive Yield Strength  5.00 MPa
@Strain 1.00 %
725 psi
@Strain 1.00 %
ISO 604 (10)
 8.50 MPa
@Strain 2.00 %
1230 psi
@Strain 2.00 %
ISO 604 (10)
 14.5 MPa
@Strain 5.00 %
2100 psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched 9.00 J/cm²42.8 ft-lb/in²Partial Break; ISO 179-1/1eA
 11.5 J/cm²54.7 ft-lb/in²Double Notched
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 2.30
@Frequency 1.00e+6 Hz
2.30
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 90.6 kV/mm2300 kV/inASTM D149
Dissipation Factor 0.000500
@Frequency 1.00e+6 Hz
0.000500
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 121 µm/m-°C67.0 µin/in-°FASTM E-831 (TMA)
 180 µm/m-°C
@Temperature 23.0 - 100 °C
100 µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity 0.400 W/m-K2.78 BTU-in/hr-ft²-°F
 0.409 W/m-K2.84 BTU-in/hr-ft²-°F
Melting Point 135 °C275 °FASTM D3418
Maximum Service Temperature, Air 79.4 °C175 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Minimum Service Temperature, Air -150 °C-238 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Targeted Usage Load + BearingLoad + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SMP16 / 20166