Mitsubishi Chemical Advanced Materials Acetron™ GP FG / Ertacetal™ C FG POM-C Copolymer Acetal, Extruded
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
;
Acetal Copolymer, Unreinforced
Material Notes:
A food grade, porosity-free copolymer acetal with greater resistance to hydrolysis, strong alkalis, and thermal oxidative degradation than homopolymer acetal grades.
Key Words:
POMC, Polyoxymethylene; Polyacetal
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Metric
English
Comments
Specific Gravity
1.41
g/cc
1.41
g/cc
ASTM D792
Water Absorption at Saturation
0.900 %
0.900 %
ASTM D570 (17)
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
84.0
84.0
ASTM D785
Hardness, Shore D
79.0
79.0
ISO 868
Tensile Strength
66.0
MPa
9570
psi
ISO 527-1/-2 (7)
Elongation at Yield
15.0 %
15.0 %
ISO 527-1/-2 (7)
Flexural Strength
91.0
MPa
13200
psi
ISO 178 (12)
Compressive Yield Strength
23.0
MPa
@Strain 1.00 %
3340
psi
@Strain 1.00 %
ISO 604 (10)
40.0
MPa
@Strain 2.00 %
5800
psi
@Strain 2.00 %
ISO 604 (10)
72.0
MPa
@Strain 5.00 %
10400
psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength
55.0
MPa
7980
psi
ASTM D732
Charpy Impact, Notched
0.800
J/cm²
3.81
ft-lb/in²
ISO 179-1/1eA
Electrical Properties
Metric
English
Comments
Surface Resistivity per Square
1.00e+14
ohm
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
3.80
@Frequency 1.00e+6 Hz
3.80
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength
16.5
kV/mm
420
kV/in
ASTM D149
20.0
kV/mm
508
kV/in
IEC 60243-1 (15)
Dissipation Factor
0.00500
@Frequency 1.00e+6 Hz
0.00500
@Frequency 1.00e+6 Hz
ASTM D150
Thermal Properties
Metric
English
Comments
CTE, linear
97.2
µm/m-°C
54.0
µin/in-°F
ASTM E-831 (TMA)
110
µm/m-°C
@Temperature 23.0 - 60.0 °C
61.1
µin/in-°F
@Temperature 73.4 - 140 °F
125
µm/m-°C
@Temperature 23.0 - 100 °C
69.4
µin/in-°F
@Temperature 73.4 - 212 °F
Thermal Conductivity
0.231
W/m-K
1.60
BTU-in/hr-ft²-°F
0.310
W/m-K
2.15
BTU-in/hr-ft²-°F
Melting Point
168
°C
335
°F
ASTM D3418
Maximum Service Temperature, Air
98.9
°C
210
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
104
°C
220
°F
ASTM D648
Minimum Service Temperature, Air
-50.0
°C
-58.0
°F
Chemical Resistance Properties
Metric
English
Comments
Acids, Strong (pH 1-3)
Acceptable
Acceptable
Acids, Weak
Limited
Limited
Alcohols
Acceptable
Acceptable
Alkalies, Strong (pH 11-14)
Acceptable
Acceptable
Alkalies, Weak
Acceptable
Acceptable
Chlorinated Solvents
Unacceptable
Unacceptable
Continuous Sunlight
Limited
Limited
Hot Water / Steam
Limited
Limited
Hydrocarbons - Aliphatic
Unacceptable
Unacceptable
Hydrocarbons - Aromatic
Unacceptable
Unacceptable
Inorganic Salt Solutions
Acceptable
Acceptable
Ketones, Esters
Unacceptable
Unacceptable
Miscellaneous Properties
Metric
English
Comments
Data Sheet Region
Americas
Americas
Targeted Usage
Load + Bearing
Load + Bearing
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.