System Message
Searches:
Step-by-Step Selector
|
Quick Database Search
(Viewing data as-entered.
Click here
to return)
Mitsubishi Chemical Advanced Materials Duratron™ T5530 PAI Compression Molded Glass Reinforced Polyamide-imide
Categories:
Polymer
;
Thermoplastic
;
Polyamide-imide (PAI)
;
Polyamide-Imide, Glass Filled
Material Notes:
A compression-molded, 30% glass reinforced PAI that offers high stiffness, strength, and creep resistance. Available in larger geometries for structural applications involving high static loads and high temperatures.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
1.61
g/cc
ASTM D792
Water Absorption at Saturation
1.50 %
ASTM D570 (17)
Mechanical Properties
Original Value
Comments
Hardness, Rockwell E
85.0
ASTM D785
Hardness, Shore D
90.0
ISO 868
Tensile Strength
125
MPa
ISO 527-1/-2 (7)
Flexural Strength
170
MPa
ISO 178 (12)
Compressive Yield Strength
55.0
MPa
@Strain 1.00 %
ISO 604 (10)
104
MPa
@Strain 2.00 %
ISO 604 (10)
190
MPa
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched
3.50
kJ/m²
ISO 179-1/1eA
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
6.30
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength
28.0
kV/mm
IEC 60243-1 (15)
700
kV/in
ASTM D149
Dissipation Factor
0.0500
@Frequency 1.00e+6 Hz
ASTM D150
Thermal Properties
Original Value
Comments
CTE, linear
26.0
µin/in-°F
ASTM E-831 (TMA)
35.0
µm/m-°C
@Temperature 23.0 - 100 °C
35.0
µm/m-°C
@Temperature 23.0 - 150 °C
40.0
µm/m-°C
@Temperature >=150 °C
Thermal Conductivity
0.360
W/m-K
2.50
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
500
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
520
°F
ASTM D648
Minimum Service Temperature, Air
-20.0
°C
Glass Transition Temp, Tg
527
°F
DMA- Tan d
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Limited
Acids, Weak
Acceptable
Alcohols
Acceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Alkalies, Weak
Limited
Chlorinated Solvents
Acceptable
Continuous Sunlight
Limited
Hot Water / Steam
Limited
Hydrocarbons - Aliphatic
Acceptable
Hydrocarbons - Aromatic
Acceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Acceptable
Miscellaneous Properties
Original Value
Comments
Data Sheet Region
Americas
Targeted Usage
Structural Uses
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.