Searches:   Step-by-Step Selector  | Quick Database Search

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ketron™ LSG PEEK-CLASSIX™ (white) Life Science Grade
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Life Science Grade PEEK stock shapes, made from Invibo PEEK-CLASSIX™ resin. Pre-assessed for biocompatibility on both resin and shape, according to USP VI and ISO 10993 for up to 30 days contact with body tissue. Exhibits high mechanical strength and stiffness, and excellent resistance to chemicals and repeated sterilization via all current methods. White color to match teeth in dental applications.

Key Words: formerly LSG PEEK-CLASSIX
Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Water Absorption at Saturation 0.450 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105ASTM D785
Tensile Strength 115 MPaISO 527-1/-2 (7)
Elongation at Yield 4.50 %ISO 527-1/-2 (7)
Compressive Yield Strength 40.0 MPa
@Strain 1.00 %
ISO 604 (10)
 79.0 MPa
@Strain 2.00 %
ISO 604 (10)
 143 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 55.0 MPaASTM D732
Charpy Impact, Notched 3.50 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 27.8 µin/in-°FASTM E-831 (TMA)
Thermal Conductivity 0.250 W/m-K
 1.74 BTU-in/hr-ft²-°F
Melting Point 644 °FASTM D3418
Maximum Service Temperature, Air 482 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 329 °FASTM D648
Minimum Service Temperature, Air -58.0 °F
 -50.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Limited
 
Miscellaneous PropertiesOriginal ValueComments
Targeted Usage Load + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.