System Message
Searches:
Step-by-Step Selector
|
Quick Database Search
Mitsubishi Chemical Advanced Materials Duratron™ T4501 PAI Polyamide-imide, compression molded bearing grade
Categories:
Polymer
;
Thermoplastic
;
Polyamide-imide (PAI)
;
Polyamide-Imide, Molded
Material Notes:
Available in larger dimensions, this grade offers excellent compressive strength and wear behavior even in harsh thermal, chemical, and stress conditions.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Metric
English
Comments
Specific Gravity
1.45
g/cc
1.45
g/cc
ASTM D792
Water Absorption at Saturation
1.50 %
1.50 %
ASTM D570 (17)
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell E
70.0
70.0
ASTM D785
Hardness, Shore D
86.0
86.0
ISO 868
Tensile Strength
110
MPa
16000
psi
ISO 527-1/-2 (7)
Flexural Strength
155
MPa
22500
psi
ISO 178 (12)
Compressive Yield Strength
39.0
MPa
@Strain 1.00 %
5660
psi
@Strain 1.00 %
ISO 604 (10)
72.0
MPa
@Strain 2.00 %
10400
psi
@Strain 2.00 %
ISO 604 (10)
130
MPa
@Strain 5.00 %
18900
psi
@Strain 5.00 %
ISO 604 (10)
Charpy Impact, Notched
0.400
J/cm²
1.90
ft-lb/in²
ISO 179-1/1eA
Electrical Properties
Metric
English
Comments
Surface Resistivity per Square
1.00e+14
ohm
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
6.00
@Frequency 1.00e+6 Hz
6.00
@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor
0.0420
@Frequency 1.00e+6 Hz
0.0420
@Frequency 1.00e+6 Hz
ASTM D150
Thermal Properties
Metric
English
Comments
CTE, linear
36.0
µm/m-°C
20.0
µin/in-°F
ASTM E-831 (TMA)
35.0
µm/m-°C
@Temperature 23.0 - 100 °C
19.4
µin/in-°F
@Temperature 73.4 - 212 °F
35.0
µm/m-°C
@Temperature 23.0 - 150 °C
19.4
µin/in-°F
@Temperature 73.4 - 302 °F
40.0
µm/m-°C
@Temperature >=150 °C
22.2
µin/in-°F
@Temperature >=302 °F
Thermal Conductivity
0.533
W/m-K
3.70
BTU-in/hr-ft²-°F
0.540
W/m-K
3.75
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
260
°C
500
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
279
°C
534
°F
ASTM D648
Minimum Service Temperature, Air
-50.0
°C
-58.0
°F
Glass Transition Temp, Tg
275
°C
527
°F
DMA- Tan d
Chemical Resistance Properties
Metric
English
Comments
Acids, Strong (pH 1-3)
Limited
Limited
Acids, Weak
Acceptable
Acceptable
Alcohols
Acceptable
Acceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Unacceptable
Alkalies, Weak
Limited
Limited
Chlorinated Solvents
Acceptable
Acceptable
Continuous Sunlight
Acceptable
Acceptable
Hot Water / Steam
Limited
Limited
Hydrocarbons - Aliphatic
Acceptable
Acceptable
Hydrocarbons - Aromatic
Acceptable
Acceptable
Inorganic Salt Solutions
Acceptable
Acceptable
Ketones, Esters
Acceptable
Acceptable
Miscellaneous Properties
Metric
English
Comments
Data Sheet Region
Americas
Americas
Targeted Usage
Load + Bearing
Load + Bearing
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
P1SM43 / 20138