Searches:   Step-by-Step Selector  | Quick Database Search

Mitsubishi Chemical Advanced Materials Ketron™ LSG CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Life Science Grade stock shapes, made from 30% carbon fiber-reinforced PEEK resin. Pre-assessed for biocompatibility on both resin and shape for up to 24 hours contact with body tissue according to USP VI and ISO 10993. Exhibits excellent mechanical strength, stiffness, resistance to chemicals and repeated sterilization via all current methods.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Water Absorption at Saturation 0.300 %0.300 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 102102ASTM D785
Hardness, Shore D 90.090.0ISO 868
Tensile Strength 144 MPa20900 psiISO 527-1/-2 (7)
Flexural Strength 220 MPa31900 psiISO 178 (12)
Compressive Yield Strength  69.0 MPa
@Strain 1.00 %
10000 psi
@Strain 1.00 %
ISO 604 (10)
 125 MPa
@Strain 2.00 %
18100 psi
@Strain 2.00 %
ISO 604 (10)
 170 MPa
@Strain 5.00 %
24700 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 103 MPa14900 psiASTM D732
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1e+05 - 1.00e+7 ohm1e+05 - 1.00e+7 ohmANSI/ESD STM 11.11
Dielectric Strength 1.26 kV/mm32.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C10.0 µin/in-°FASTM E-831 (TMA)
 25.0 µm/m-°C
@Temperature 23.0 - 100 °C
13.9 µin/in-°F
@Temperature 73.4 - 212 °F
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
13.9 µin/in-°F
@Temperature 73.4 - 302 °F
 55.0 µm/m-°C
@Temperature >=150 °C
30.6 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.920 W/m-K6.38 BTU-in/hr-ft²-°F
 0.922 W/m-K6.40 BTU-in/hr-ft²-°F
Melting Point 340 °C644 °FASTM D3418
Maximum Service Temperature, Air 250 °C482 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 270 °C518 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Targeted Usage Load + BearingLoad + Bearing
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.