Material Notes: |
Produced from recycled industrial grade UHMW-PE, TIVAR™ ECO offers excellent performance coupled with cost-effectiveness and eco-friendliness. A favored solution for wear and outrigger pads, strips, rails, and guides, rollers, conveyors, chutes, hoppers, impact plates, and asphalt equipment components.
|