Mitsubishi Chemical Advanced Materials Nylatron™ MC™ 907 / Ertalon™ 6 PLA PA6 Unfilled Type 6 nylon
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Cast
Material Notes:
An unmodified cast nylon 6 with great mechanical and electrical insulation properties, as well as resistance to creep, wear, fatigue, heat aging, and radiation.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
1.15
g/cc
ASTM D792
Water Absorption at Saturation
7.00 %
ASTM D570 (17)
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
88.0
ASTM D785
Hardness, Shore D
80.0
ISO 868
Tensile Strength
88.0
MPa
ISO 527-1/-2 (7)
Elongation at Yield
5.00 %
ISO 527-1/-2 (7)
Flexural Strength
121
MPa
ISO 178 (12)
Compressive Yield Strength
34.0
MPa
@Strain 1.00 %
ISO 604 (10)
64.0
MPa
@Strain 2.00 %
ISO 604 (10)
93.0
MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength
76.0
MPa
ASTM D732
Charpy Impact, Notched
3.00
kJ/m²
ISO 179-1/1eA
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
1.00e+14
ohm
ANSI/ESD STM 11.11
Dielectric Constant
3.70
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength
25.0
kV/mm
IEC 60243-1 (15)
500
kV/in
ASTM D149
Thermal Properties
Original Value
Comments
CTE, linear
50.0
µin/in-°F
ASTM E-831 (TMA)
80.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
90.0
µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity
0.290
W/m-K
1.70
BTU-in/hr-ft²-°F
Melting Point
420
°F
ASTM D3418
Maximum Service Temperature, Air
200
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
200
°F
ASTM D648
Minimum Service Temperature, Air
-30.0
°C
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Unacceptable
Acids, Weak
Limited
Alcohols
Limited
Alkalies, Strong (pH 11-14)
Unacceptable
Alkalies, Weak
Limited
Chlorinated Solvents
Limited
Continuous Sunlight
Limited
Hot Water / Steam
Limited
Hydrocarbons - Aliphatic
Acceptable
Hydrocarbons - Aromatic
Acceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Acceptable
Miscellaneous Properties
Original Value
Comments
Data Sheet Region
Americas
Targeted Usage
Load + Bearing
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.