Mitsubishi Chemical Advanced Materials Nylatron™ GSM Blue PA6 Cast Oil & MoS2 Filled Type 6
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, MoS2 Filled
Material Notes:
Nylatron™ GSM Blue Polyamide PA6 is a Molybdenum Disulfide (MoS2) and oil filled nylon that is characterized by its superior frictional characteristics, low coefficient of friction, greater limiting PV, and low “k” factor.
Key Words:
Polyamide 6; PA6; PA 6
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
1.15
g/cc
ASTM D792
Water Absorption at Saturation
6.00 %
ASTM D570 (17)
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
1.00e+14
ohm
ANSI/ESD STM 11.11
Thermal Properties
Original Value
Comments
CTE, linear
55.0
µin/in-°F
ASTM E-831 (TMA)
Melting Point
420
°F
ASTM D3418
Maximum Service Temperature, Air
200
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
200
°F
ASTM D648
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Limited
Acids, Weak
Limited
Alcohols
Acceptable
Alkalies, Strong (pH 11-14)
Acceptable
Alkalies, Weak
Acceptable
Chlorinated Solvents
Acceptable
Continuous Sunlight
Acceptable
Hot Water / Steam
Limited
Hydrocarbons - Aliphatic
Acceptable
Hydrocarbons - Aromatic
Acceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Acceptable
Miscellaneous Properties
Original Value
Comments
Data Sheet Region
Americas
Targeted Usage
Load + Bearing
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.