Searches:   Step-by-Step Selector  | Quick Database Search

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Duratron™ T7530 PAI Compression Molded Carbon Fiber Reinforced Polyamide-Imide
Categories: Polymer; Thermoplastic; Polyamide-imide (PAI)

Material Notes: A compression molded, 30% carbon fiber-reinforced polyamide-imide with outstanding strength and stiffness, as well as the lowest coefficient of thermal expansion of all PAI materials.

Key Words: Duratron, T7530 PAI, Polyamide-imide (Torlon)
Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Water Absorption at Saturation 1.50 %ASTM D570 (17)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°FASTM E-831 (TMA)
Thermal Conductivity 3.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °FContinuous Use Temperature in Air after 20000 hr
Glass Transition Temp, Tg 527 °FDMA- Tan d
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Acceptable
Continuous Sunlight Acceptable
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.