System Message
Searches:
Step-by-Step Selector
|
Quick Database Search
(Viewing data as-entered.
Click here
to return)
Mitsubishi Chemical Advanced Materials Proteus™ HDPE Black High Density Polyethylene Black
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
Material Notes:
These black, high density PE shapes exhibit excellent impact resistance, superior tensile strength, low moisture absorption, great chemical and corrosion resistance, and easy fabrication and welding capabilities.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Original Value
Comments
Specific Gravity
0.960
g/cc
ASTM D792
Water Absorption at Saturation
<= 0.0100 %
ASTM D570 (17)
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
1.00e+15
ohm
ANSI/ESD STM 11.11
Thermal Properties
Original Value
Comments
CTE, linear
67.0
µin/in-°F
ASTM E-831 (TMA)
Melting Point
260
°F
ASTM D3418
Maximum Service Temperature, Air
180
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
176
°F
ASTM D648
Chemical Resistance Properties
Original Value
Comments
Acids, Strong (pH 1-3)
Unacceptable
Acids, Weak
Acceptable
Alcohols
Acceptable
Alkalies, Strong (pH 11-14)
Unacceptable
Alkalies, Weak
Acceptable
Chlorinated Solvents
Limited
Continuous Sunlight
Limited
Hot Water / Steam
Limited
Hydrocarbons - Aliphatic
Acceptable
Hydrocarbons - Aromatic
Acceptable
Inorganic Salt Solutions
Acceptable
Ketones, Esters
Acceptable
Miscellaneous Properties
Original Value
Comments
Targeted Usage
Structural Uses
Descriptive Properties
ESd category
Insulative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.