Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 61.061.0ISO 868
Tensile Strength 20.0 MPa2900 psiISO 527-1/-2 (7)
Elongation at Yield 16.0 %16.0 %ISO 527-1/-2 (7)
Flexural Strength 20.0 MPa2900 psiISO 178 (12)
Compressive Yield Strength  6.80 MPa
@Strain 1.00 %
986 psi
@Strain 1.00 %
ISO 604 (10)
 10.7 MPa
@Strain 2.00 %
1550 psi
@Strain 2.00 %
ISO 604 (10)
 17.2 MPa
@Strain 5.00 %
2490 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 23.0 MPa3340 psiASTM D732
Charpy Impact, Notched 10.6 J/cm²50.4 ft-lb/in²Partial Break; ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+13 ohm1.00e+13 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 144 µm/m-°C80.0 µin/in-°FASTM E-831 (TMA)
Melting Point 135 °C275 °FASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Minimum Service Temperature, Air -200 °C-328 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Load + BearingLoad + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SMP13c / 161709