Mitsubishi Chemical Advanced Materials Nylatron™ Nylon 105 PA66 Black PA66 Black
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: This PA66 grade exhibits an ideal balance of strength, toughness, and wear resistance. This versatile, high-performance nylon material offers broad size and shape availability and is commonly used for general purpose bearing and wear components.

Key Words: Extruded, UV Stabilized, Nylon 66
Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/ccASTM D792
Water Absorption at Saturation 7.00 %ASTM D570 (17)
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.60
@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.0300
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.70 BTU-in/hr-ft²-°F
Melting Point 500 °FASTM D3418
Maximum Service Temperature, Air 175 °FContinuous Use Temperature in Air after 20000 hr
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.