Mitsubishi Chemical Advanced Materials Ketron™ Sterra™ HPV PEEK Recycled poly-ether-ether-ketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Carbon fiber reinforced with graphite and PTFE lubricants, a recycled PEEK grade with the lowest coefficient of friction and the best machinability.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.44 g/cc1.44 g/ccASTM D792
Water Absorption at Saturation 0.300 %0.300 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 85.085.0ASTM D785
Hardness, Shore D 86.086.0ISO 868
Tensile Strength 78.0 MPa11300 psiISO 527-1/-2 (7)
Flexural Strength 125 MPa18100 psiISO 178 (12)
Compressive Yield Strength  46.0 MPa
@Strain 1.00 %
6670 psi
@Strain 1.00 %
ISO 604 (10)
 80.0 MPa
@Strain 2.00 %
11600 psi
@Strain 2.00 %
ISO 604 (10)
 120 MPa
@Strain 5.00 %
17400 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 69.0 MPa10000 psiASTM D732
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.6 µm/m-°C17.0 µin/in-°FASTM E-831 (TMA)
 35.0 µm/m-°C
@Temperature 23.0 - 100 °C
19.4 µin/in-°F
@Temperature 73.4 - 212 °F
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
22.2 µin/in-°F
@Temperature 73.4 - 302 °F
 85.0 µm/m-°C
@Temperature >=150 °C
47.2 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.245 W/m-K1.70 BTU-in/hr-ft²-°F
 0.780 W/m-K5.41 BTU-in/hr-ft²-°F
Melting Point 340 °C644 °FASTM D3418
Maximum Service Temperature, Air 250 °C482 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 195 °C383 °FASTM D648
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Load + BearingLoad + Bearing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.