Mitsubishi Chemical Advanced Materials Semitron™ ESd 410C PEI Static Dissipative Polyetherimide
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Semitron™ ESd 410C is an electrostatic dissipative PEI material that exhibits excellent dimensional stability characteristics and resistance to extreme temperatures, ideal for semiconductor and electronics handling.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Water Absorption at Saturation 1.10 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 115ASTM D785
Hardness, Shore D 85.0ISO 868
Tensile Strength 62.0 MPaISO 527-1/-2 (7)
Flexural Strength 80.0 MPaISO 178 (12)
Compressive Yield Strength 44.0 MPa
@Strain 1.00 %
ISO 604 (10)
 76.0 MPa
@Strain 2.00 %
ISO 604 (10)
 114 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 62.0 MPaASTM D732
Charpy Impact, Notched 4.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 10000 ohmANSI/ESD STM 11.11
Dielectric Constant 3.00
@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.00130
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µin/in-°FASTM E-831 (TMA)
 40.0 µm/m-°C
@Temperature 23.0 - 100 °C
 40.0 µm/m-°C
@Temperature 23.0 - 150 °C
 45.0 µm/m-°C
@Temperature >=150 °C
Thermal Conductivity 0.350 W/m-K
 2.45 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 338 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 410 °FASTM D648
Glass Transition Temp, Tg 410 °FDMA- Tan d
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Continuous Sunlight Acceptable
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Limited
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Miscellaneous PropertiesOriginal ValueComments
Data Sheet Region Americas
Targeted Usage Structural Uses
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.