Mitsubishi Chemical Advanced Materials Nylatron™ NSM PA6 Nylon, Cast Solid Lubricant Filled, Type 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Fiber/Solid Lube Filled

Material Notes: The most wear-resistant nylon available, this self-lubricating cast nylon has a dynamic load-bearing capacity up to five times higher and a service life up to 10 times longer than conventional cast nylons.

Key Words: Polyamide 6; PA6; PA 6
Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Water Absorption at Saturation 7.00 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 81.0ASTM D785
Hardness, Shore D 76.0ISO 868
Tensile Strength 80.0 MPaISO 527-1/-2 (7)
Elongation at Yield 5.00 %ISO 527-1/-2 (7)
Flexural Strength 109 MPaISO 178 (12)
Compressive Yield Strength 31.0 MPa
@Strain 1.00 %
ISO 604 (10)
 59.0 MPa
@Strain 2.00 %
ISO 604 (10)
 87.0 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 69.0 MPaASTM D732
Charpy Impact, Notched 3.50 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Strength 25.0 kV/mmIEC 60243-1 (15)
 400 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µin/in-°FASTM E-831 (TMA)
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 95.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.290 W/m-K
Melting Point 420 °FASTM D3418
Maximum Service Temperature, Air 200 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 200 °FASTM D648
Minimum Service Temperature, Air -30.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Limited
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Miscellaneous PropertiesOriginal ValueComments
Data Sheet Region Americas
Targeted Usage Load + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.