Searches:   Step-by-Step Selector  | Quick Database Search

Mitsubishi Chemical Advanced Materials Fluorosint™ HPV PTFE Mica-filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Fluorosint™ HPV is an FDA compliant, high-performance, bearing grade PTFE material. Optimized for high-pressure velocity and low k-factor, Fluorosint™ HPV was developed specifically for bearing applications where other PTFE formulations typically exhibit premature wear.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.06 g/cc2.06 g/ccASTM D792
Water Absorption at Saturation 0.430 %0.430 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 45.045.0ASTM D785
Hardness, Shore D 64.064.0ISO 868
Tensile Strength 10.0 MPa1450 psiISO 527-1/-2 (7)
Elongation at Yield 6.00 %6.00 %ISO 527-1/-2 (7)
Flexural Strength 18.0 MPa2610 psiISO 178 (12)
Compressive Yield Strength  10.0 MPa
@Strain 1.00 %
1450 psi
@Strain 1.00 %
ISO 604 (10)
 14.5 MPa
@Strain 2.00 %
2100 psi
@Strain 2.00 %
ISO 604 (10)
 19.0 MPa
@Strain 5.00 %
2760 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 17.0 MPa2470 psiASTM D732
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 88.2 µm/m-°C49.0 µin/in-°FASTM E-831 (TMA)
 75.0 µm/m-°C
@Temperature 23.0 - 100 °C
41.7 µin/in-°F
@Temperature 73.4 - 212 °F
 80.0 µm/m-°C
@Temperature 23.0 - 150 °C
44.4 µin/in-°F
@Temperature 73.4 - 302 °F
 135 µm/m-°C
@Temperature >=150 °C
75.0 µin/in-°F
@Temperature >=302 °F
Melting Point 327 °C621 °FASTM D3418
Maximum Service Temperature, Air 260 °C500 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FASTM D648
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) UnacceptableUnacceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Miscellaneous PropertiesMetricEnglishComments
Data Sheet Region AmericasAmericas
Targeted Usage Load + BearingLoad + Bearing
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

P1SM09M / 20083