Mitsubishi Chemical Advanced Materials Techtron™ GF40 PPS Polyphenylene Sulfide
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Techtron™ GF40 is a 40% glass fiber reinforced grade of PPS that exhibits higher stiffness and creep resistance than other PPS grades. Because of its improved dimensional stability, this grade excels in structural applications involving a high static load, even for long periods of time and at elevated temperatures.

Printer friendly version Printer friendly version  PDF Download Download as PDF  Add to Folder:
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90.0ASTM D785
Tensile Strength 60.0 MPaISO 527-1/-2 (7)
Charpy Impact, Notched 5.50 kJ/m²ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
@Temperature 23.0 - 100 °C
 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
 65.0 µm/m-°C
@Temperature >=150 °C
Melting Point 540 °FASTM D3418
Minimum Service Temperature, Air -20.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Limited
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.