System Message
Searches:
Step-by-Step Selector
|
Quick Database Search
Mitsubishi Chemical Advanced Materials Techtron™ PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Sulfide (PPS)
;
Polyphenylene Sulfide (PPS); Molded
Material Notes:
Techtron™ PSBG PPS compression molded shapes are internally lubricated and carbon fiber-reinforced, allowing them to exhibit excellent wear resistance, outstanding dimensional stability, and extreme chemical and corrosion resistance.
Printer friendly version
Download as PDF
Add to Folder:
My Folder
-- task --
Export to Solidworks
Export to ALGOR
Export to ANSYS
Export to NEiWorks
Export to COMSOL
Export to ETBX
Export to SpaceClaim
Physical Properties
Metric
English
Comments
Specific Gravity
1.52
g/cc
1.52
g/cc
ASTM D792
Water Absorption at Saturation
0.0300 %
0.0300 %
ASTM D570 (17)
Electrical Properties
Metric
English
Comments
Surface Resistivity per Square
1e+05
1e+05
ANSI/ESD STM 11.11
Thermal Properties
Metric
English
Comments
CTE, linear
30.6
µm/m-°C
17.0
µin/in-°F
ASTM E-831 (TMA)
Thermal Conductivity
0.255
W/m-K
1.77
BTU-in/hr-ft²-°F
Melting Point
282
°C
540
°F
ASTM D3418
Maximum Service Temperature, Air
221
°C
430
°F
Continuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi)
254
°C
490
°F
ASTM D648
Chemical Resistance Properties
Metric
English
Comments
Acids, Strong (pH 1-3)
Limited
Limited
Acids, Weak
Acceptable
Acceptable
Alcohols
Acceptable
Acceptable
Alkalies, Strong (pH 11-14)
Acceptable
Acceptable
Alkalies, Weak
Acceptable
Acceptable
Chlorinated Solvents
Acceptable
Acceptable
Continuous Sunlight
Limited
Limited
Hot Water / Steam
Acceptable
Acceptable
Hydrocarbons - Aliphatic
Acceptable
Acceptable
Hydrocarbons - Aromatic
Acceptable
Acceptable
Inorganic Salt Solutions
Acceptable
Acceptable
Ketones, Esters
Acceptable
Acceptable
Miscellaneous Properties
Metric
English
Comments
Data Sheet Region
Americas
Americas
Targeted Usage
Load + Bearing
Load + Bearing
Descriptive Properties
ESd category
Dissipative
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
P1SM36A / 20129