Searches:   Step-by-Step Selector  | Quick Database Search
Ensinger PEI
Mitsubishi Chemical Advanced Materials TIVAR™ Extended Wear UHMW-PE, Premium Glass-filled, Partially Cross-linked
Categories: Polymer; Thermoplastic; Polyethylene (PE); UHMW-PE

Material Notes: TIVAR™ Extended Wear is a glass filled and partially cross-linked UHMW-PE. This modified formula retains all the key properties of TIVAR™ including low friction surface, wear and corrosion resistance, and impact strength.

Key Words: formerly TIVAR® Extended Wear UHMW-PE
Available Properties
  • Specific Gravity
  • Hardness, Shore D
  • Tensile Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Shear Strength
  • Charpy Impact, Notched
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Minimum Service Temperature, Air
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  • Targeted Usage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.