Searches:   Step-by-Step Selector  | Quick Database Search
Ensinger PEI
Mitsubishi Chemical Advanced Materials Proteus™ LSG HS PP-H Heat Stabilized Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Life Science Grade, Heat Stabilized PP-H stock shapes, made from high purity homopolymer polypropylene resin. Shapes are pre-assessed for biocompatibility at the stock shape level (USP VI & ISO 10993) and are supported for use in non-body contact medical applications. Exhibits superior resistance to steam sterilization, cleaning agents, and disinfectants over standard PP materials, and has improved dimensional stability.

Available Properties
  • Specific Gravity
  • Tensile Strength
  • Elongation at Yield
  • Flexural Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Compressive Yield Strength
  • Charpy Impact, Notched
  • Surface Resistivity per Square
  • CTE, linear
  • Melting Point
  • Maximum Service Temperature, Air
  • USP Class VI
  • Acids, Strong (pH 1-3)
  • Acids, Weak
  • Alcohols
  • Alkalies, Strong (pH 11-14)
  • Alkalies, Weak
  • Chlorinated Solvents
  • Continuous Sunlight
  • Hot Water / Steam
  • Hydrocarbons - Aliphatic
  • Hydrocarbons - Aromatic
  • Inorganic Salt Solutions
  • Ketones, Esters
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's disclaimer and terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.